EN8 vs EN9 vs EN19 vs EN24: Which Steel Grade Do You Need?
Navdeesh Kandhari
9 minutes reading
Nov 23, 2026

EN8, EN9, EN19 and EN24 are four of the most commonly specified engineering steels in India. They look similar on a drawing, but they differ a lot in strength, hardenability, machinability and price. Choosing a higher grade than you need wastes money; choosing a lower one risks failure in service. This guide compares the four side by side.
A quick note on EN grades
EN numbers come from the old British Standard BS 970. Newer designations exist (for example 080M40 for EN8), but the EN names are still what most buyers and machinists use in India. Each grade also has close international equivalents, which helps when you are working from a foreign drawing.
Composition at a glance
Grade | Type | Carbon (%) | Key alloying elements | Close equivalents |
|---|---|---|---|---|
EN8 | Medium carbon steel | 0.36 to 0.44 | Manganese only | 080M40, C40/C45, AISI 1040 |
EN9 | Higher carbon steel | 0.50 to 0.60 | Manganese only | 070M55, C55, AISI 1055 |
EN19 | Alloy steel | 0.35 to 0.45 | Chromium, molybdenum | 709M40, 42CrMo4, AISI 4140 |
EN24 | Alloy steel | 0.36 to 0.44 | Nickel, chromium, molybdenum | 817M40, 34CrNiMo6, AISI 4340 |
Strength and hardenability
Strength depends heavily on the condition the steel is supplied in (as rolled, normalised, or hardened and tempered). As a broad guide, the grades rank in this order:
Grade | Typical tensile strength range (N/mm2) | Through-hardening |
|---|---|---|
EN8 | About 550 to 850 | Limited, mainly surface or small sections |
EN9 | About 650 to 850 | Limited, good surface hardness |
EN19 | About 700 to 1,000+ | Good in medium sections |
EN24 | About 850 to 1,300 | Excellent, even in large sections |
Hardenability is the key difference. Plain carbon steels like EN8 and EN9 only harden to a shallow depth, so large sections stay soft in the middle. The chromium and molybdenum in EN19, and the added nickel in EN24, let the steel harden through thicker sections and give better toughness.
EN8: the everyday engineering steel
EN8 is the default choice for general engineering parts that need more strength than mild steel but no special treatment. It machines well in the bright drawn condition and can be flame or induction hardened on the surface. Typical uses: shafts, axles, studs, bolts, pins, couplings and spindles.
EN9: when wear resistance matters
With higher carbon, EN9 reaches a harder surface than EN8 after hardening, which makes it better for parts that rub or wear. Typical uses: sprockets, cams, gears, rollers and wear plates.
EN19: high tensile for loaded parts
EN19 is the go-to alloy steel when a part must carry high loads or shock. It is usually supplied hardened and tempered. Typical uses: high-tensile bolts and studs, crankshafts, gears, axle shafts and heavy-duty fasteners.
EN24: for the toughest applications
EN24 combines high strength with excellent toughness, even in large sections. It costs more and is harder to machine, so it is used only where the duty demands it. Typical uses: heavy-duty shafts, gears, connecting rods, aircraft and defence components, and highly stressed machine parts.
How to choose
Start with the load. If EN8 is strong enough, there is no reason to pay for an alloy grade.
Consider section size. For large diameters that must be hardened through, choose EN19 or EN24.
Consider wear. If surface hardness matters more than core strength, EN9 can be a cost-effective choice.
Check machining cost. Higher grades take longer to machine and wear tools faster.
Specify the condition. 'EN19 hardened and tempered to R condition' is a complete specification. 'EN19' alone is not.
Machinability and cost
Machinability falls and price rises as you move from EN8 to EN24. EN8 in the bright drawn condition is easy to turn, drill and thread. EN9 is slightly harder on tools. EN19 and EN24, especially when supplied hardened and tempered, need slower speeds, rigid set-ups and better tooling. When comparing quotes for a machined part, include the extra machining time, not just the cost of the bar.
Ordering these grades as bright bars
All four grades can be supplied as cold drawn bright bars in round, and some in hex and square. When you order, specify the grade, the supply condition, the size and tolerance class (h9, h10 or h11), the length and the quantity, and ask for a mill test certificate showing chemical composition and mechanical properties. That one line on the order saves arguments later.
Frequently asked questions
Is EN19 the same as AISI 4140?
They are close equivalents with very similar chromium molybdenum chemistry. 42CrMo4 is the European equivalent. Always check the exact composition and condition on the mill test certificate.
Which is stronger, EN8 or EN19?
EN19. As an alloy steel, it reaches much higher strength and toughness after heat treatment, and it hardens through thicker sections than EN8.
Can EN8 be hardened?
Yes, but mainly at the surface, by flame or induction hardening. Because it is a plain carbon steel, large EN8 sections do not harden through to the core.
Not sure which grade suits your part? Send us the drawing and duty, and we'll suggest a grade and size. Send your requirement on WhatsApp: +91 7065337337, or browse the range on ssengineeringwork.in.